教学文库网 - 权威文档分享云平台
您的当前位置:首页 > 精品文档 > 高等教育 >

碳纤维增强SiC陶瓷复合材料的研究进展(精)(4)

来源:网络收集 时间:2026-09-04
导读: [40-41] [16] [39] Composites:part A, 2001,31: 133-142. [3] D.H.BAHLOUL. The role of chemistry in the synthesis of ceramic materials[J]. Key Eng.Mater. 206-213, 2002:15-20. [4] T.TANAKA, N.TAMARI, e

[40-41] [16] [39]

Composites:part A, 2001,31: 133-142.

[3] D.H.BAHLOUL. The role of chemistry in the synthesis of ceramic materials[J]. Key Eng.Mater. 206-213, 2002:15-20.

[4] T.TANAKA, N.TAMARI, et al. Fabrication of three-dimensional tyranno fibre reinforced SiC composite by the polymer precursor method[J]. Ceram.International 1998,24: 365-370.

[5] Z.S.RAK. A process for Cf /SiC composites using liquid polymer infiltration[J]. J.Am.Ceram.Soc. 2001,84:2 235-2 239. [6] NYAN-HWA TAI, CHE-FU CHEN. Nanofiber formation 。

最近,碳纤维增强 SiC 陶瓷复合材料又用于卫星反射镜坏体的制备,美、俄、德等国在这方面都有研究,德国已经研制成功商业用 Cf/SiC反射镜,其镜面直径为 36cm。各国正在发展的碳纤

第二期 邹世钦, 等:炭纤维增强SIC 陶瓷复合材料的研究进展- 19 -

in the fabrication of carbon/silicon carbide ceramic matrix nanocomposites by slurry impregnation and pulse chemical vapor infiltration[J]. J.Am.Ceram.Soc.2001,84: 1 683-1 688.

[7] BYUNG JUN OH, YOUNG JIN LEE,et al. Fabrication

of carbon/silicon carbide composites by isothermal chemical vapor infiltration, using the in situ whisker-growing and matrix-filling process[J]. J.Am.Ceram.Soc.2001,84: 245-247.

[8] JINGYI DENG, YONGLIANG WEi,et al. Carbon-fiber-reinforced composites with graded carbon-silicon carbide matrix composition[J]. J.Am.Ceram.Soc. 1999,82: 1 629-1632.

[9] YONGDONG XU, LITONG ZHANG,et al. Microstructure

and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration[J]. Carbon, 1998,36: 1 051-1 056.

[10] WENCHUAN LIU, YONGLIANG WEI,et al. Carbon-fiber-reinforced C-SiC binary matrix composites[J].carbon, 1995,33: 441-447. [11] , 曹英斌张长瑞, 等. Cf /SiC陶瓷基复合材料发展状况[J].宇航材料工艺, 1999(5: 10-14.

[12] D.KLOSTERMAN, R.CHARTOFF,et al. Laminated

object manufacturing, a New Process for the Direct Manufacture of Monolithic Ceramics and Continuous Fiber CMCs[J]. Ceram.Eng.& Sci.Proceedings, 1997,18(4: 113-120.

[13] M.M.ANGELOVICI, R.G.BRYANT,et al. Carbon/

ceramic microcomposites, preparation and properties[J].Mater.Lett, 1998,36: 254-265.

[14] E.VOGLI, J.MUKERJI,et al. Conversion of oak to

cellular silicon carbide ceramic by gas-phase reaction with silicon monoxide[J]. J.Am.Ceram.Soc. 2001,84:1 236-1 240.

[15] . CMC(网村清人セラミツクス基复合材料[J]. 日本复 合材料学会志, 1994,20: 34-41.

[16] J.S.FISCHEDICK, A.ZERN,et al. The morphology of

silicon carbide in C/C-SiC composites[J]. Mater.Sci.& Eng.A, 2002,332: 146-152. [17] DONG-WOO SHIN, SAM-SHIK PARK,et al. Silicon/

silicon carbide composites fabricated by infiltration of a silicon melt into charcoal[J]. J.Am.Ceram.Soc. 1999,82:3 251-3 253.

[18] H.LEITE, U.DAMBACHER,et al. Microstructure and properties of multilayer coatings iwth covalent bonded hard materials[J]. Surf.Coat.Tech.116-119, 1999: 313-320. [19] Z.FAN, Y.Song,et al. Oxidation behavior of fine-

grained SiC-B4C/C composites up to 1400 oC[J].Carbon, 2003,41: 429-436. [20] M.APARICIO, A.DURAN,et al. Yttrium silicate

coatings for oxidation protection of carbon silicon carbide composites[J]. J.Am.Ceram.Soc. 2000,83:1 351-1 355.

[21] J.D.WEBSTER, M.E.WESTWOOD,et al. Oxidation

protection coatings for C/SiC based on yttrium silicate[J]. J.Eur.Ceram.Soc. 1998,18: 2 345-2 350.[22] LAIFEI CHENG, YONGDONG XU,et al. Effect of

carbon interlayer on oxidation behavior of C/SiC composites with a coating from room temperature to

1500℃[J]. Mater.Sci.Eng.A, 2001,300: 219-225. [23] LAIFEI CHENG, YONGDONG XU,et al. Oxidation

and defect control of CVD SiC coating on three-dimensional C/SiC composites[J]. Carbon, 2002,40: 2 229-2 234.

[24] LAIFEI CHENG, YONGDONG XU,et al. Effect of

glass sealing on the oxidation behavior of three dimensional C/SiC composites in air[J]. Carbon,2001,39: 1 127-1 133.

[25] J.D.WEBSTER, F.H.HAYES,et al. Thermodynamic

modelling and experimental studies in the design of integrated oxidation protection systems for ceramic matrix composites[J]. Key.Eng.Mater.127-131,

1997: 1 225-1 232.

[26] M.E.WESTWOOD, R.J.DAY,et al. The use of finite element analysis in the design of integrated oxidation

protection systems for ceramic matrix composites[J].Key.Eng.Mater.127-131, 1997: 1 233-1 240.

[27] LAIFEI CHENG, YONGDONG XU,et al. Oxidation

behavior of C-SiC composites with a Si-W coating from room temperature to 1500℃[J]. Carbon, 2000,38: 2 133-2 138.

[28] , 刘荣军周新贵, 等. CVD法制备SiC 先进陶瓷材料研 究进展[J]. , 2002(7: 46材料工程-49.

[29] S.GOUJARD, L.VANDENBULCKE,et al. The

oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings[J].J.Mater.Sci. 1994,29: 6 212-6 220.

[30] L.D.BENTSON, R.J.PRICE,et al. Moisture and oxidation resistant carbon/carbon composites[P]. 美国专利:5298311, 1994-03-29.

[31] H.FRITZE, J.JOJIC,et al. Mullite based oxidation

protection for SiC-C/C composites in air at temperatures up to 1900 K[J]. J.Eur.Ceram.Soc.1998,18: 2 351

-2 364.

- 20 - 高科技纤维与应用 243. 第二十八卷 [32] H.FRITZE, J.JOJIC,et al. Mullite based oxidation protection for SiC-C/C composites in Air at temperatures up to 1900 K[J]. Key.Eng. Mater. 132136, 1997: 1 629- 1 632. [33] R.NASLAIN, R.PAILLER,et al. Processing of ceramic matrix composites by pulsed-CVI and related techniques[J]. Key.Eng.Mater.206-213, 2002: 2 189-2 192. [34] F.LAMOUROUX, S.BERTRAND,et al. Oxidationresistant carbon-fiber-reinforced ceramic-matrix composites[J].

Compos.Sci.Tech. 1999,59: 1 073 - 1 085. [35] 张建艺 . 陶瓷基复合材料在喷管 …… 此处隐藏:4283字,全部文档内容请下载后查看。喜欢就下载吧 ……

碳纤维增强SiC陶瓷复合材料的研究进展(精)(4).doc 将本文的Word文档下载到电脑,方便复制、编辑、收藏和打印
本文链接:https://www.jiaowen.net/wendang/613712.html(转载请注明文章来源)
Copyright © 2020-2025 教文网 版权所有
声明 :本网站尊重并保护知识产权,根据《信息网络传播权保护条例》,如果我们转载的作品侵犯了您的权利,请在一个月内通知我们,我们会及时删除。
客服QQ:78024566 邮箱:78024566@qq.com
苏ICP备19068818号-2
Top
× 游客快捷下载通道(下载后可以自由复制和排版)
VIP包月下载
特价:29 元/月 原价:99元
低至 0.3 元/份 每月下载150
全站内容免费自由复制
VIP包月下载
特价:29 元/月 原价:99元
低至 0.3 元/份 每月下载150
全站内容免费自由复制
注:下载文档有可能出现无法下载或内容有问题,请联系客服协助您处理。
× 常见问题(客服时间:周一到周五 9:30-18:00)